Silver Art Clay
Posted: Tue Apr 01, 2003 3:00 pm
by Judi R
Does anyone out there know of a good source for silver art clay? There's a low-temp version that fuses at glass-fusing temps - but I'm finding all sources to be around the same price, $14 - $19 for 10 gr. Any ideas?

Re: Silver Art Clay
Posted: Tue Apr 01, 2003 3:41 pm
by dee
jjrentschler wrote:Does anyone out there know of a good source for silver art clay? There's a low-temp version that fuses at glass-fusing temps - but I'm finding all sources to be around the same price, $14 - $19 for 10 gr. Any ideas?

it's expensive stuff - pmc 3 fires at the lowest temp and pmc + is lower than the original if i remember correctly, try aaproducts.com, so far i have found they have the best pricing on this stuff....
D
Posted: Tue Apr 01, 2003 4:11 pm
by KatyPattison
Have you tried
http://www.artclayworld.com? They have a store and you can purchase all their products on line.
I still like ACS more than PMC for glass because it still shrinks less than their PMC (3 or + I can't remember which is the equivalent). Personal preference only.