Page 1 of 1
					
				anyone have a picture of an item made with b.e. 1126?
				Posted: Thu Jan 22, 2004 2:38 pm
				by charlie
				it's one of the new hot colors, but the picture on the b.e. site for it is underwhelming.
			 
			
					
				
				Posted: Thu Jan 22, 2004 3:28 pm
				by SAReed
				I have a sample of the unfused color.  It's a greenish medium amber.  And it's as underwhelming in person as in the picture.  I can't wait to see what can be done with it, I'm sure someone here can make it beautiful.
			 
			
					
				
				Posted: Thu Jan 22, 2004 4:07 pm
				by Barbara Muth
				Charlie, I have run a couple of tests with it.  So far I am not jumping for joy.  And I love chartreuse!  Next I am going to try using it over spring green, see if it takes the green down a notch or two.  will post test results after that.