Float glass devitrification spray or other technique

Posted: Tue Jan 27, 2004 8:36 pm
by Felt Glass
Anyone have technique for avoiding devit on float glass at 1600f?

Posted: Thu Jan 29, 2004 11:00 am
by hoknok
Borax (20 mule team) mixed with water and spayed on the glass. To this date, I have not had any devit problems so far.

Devit

Posted: Thu Jan 29, 2004 8:17 pm
by Felt Glass
Thanks Hoknok, I'll give it a try.

Re: Float glass devitrification spray or other technique

Posted: Fri Jan 30, 2004 2:17 pm
by nancy burke
Felt Glass wrote:Anyone have technique for avoiding devit on float glas
s at 1600f?


I use 'Clear Coat Overglaze" which is ideal for clear window
glass or plate
OR
Super Spray. Both these Fuse Master products come from Gil Reynolds
Fusion Headquarters. I consider both to be never-fails.

p.s.
Usually, I spray these products on.

neb