I think I read in here that Welders (industrial) had the best results for gluing bails to pendants. So which do I use? Welders or E6000?
Thanks to all you pros for the wealth of information on this board!
which glue for pendants
Moderators: Brad Walker, Tony Smith
-
Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
Re: which glue for pendants
Search the archives on "E6000", "Loctite" and "Epoxy" -- there is a ton of information in past threads.
- Paul
- Paul
Lyn wrote:I think I read in here that Welders (industrial) had the best results for gluing bails to pendants. So which do I use? Welders or E6000?
Thanks to all you pros for the wealth of information on this board!
-
Alecia Helton
- Posts: 108
- Joined: Mon Aug 25, 2003 12:35 am
- Location: outside of Dallas TX
-
Gale aka artistefem
- Posts: 184
- Joined: Sun Mar 09, 2003 8:14 pm
- Location: MO-on the banks of the Mississippi
- Contact: