Flower former too high for kiln?
Moderator: Tony Smith
-
Pat Reynolds
- Posts: 6
- Joined: Mon May 28, 2012 12:23 am
Flower former too high for kiln?
My kiln is 11" deep, with top and side heating elements. I have a 7" high flower former I would like to use. Allowing for kiln shelf and 1" posts, does this leave the glass too close to the heating element? This is probably an elementary question but have just purchased this kiln and am still at the "know nothing" stage.
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Flower former too high for kiln?
Take out the kiln shelf and place the flower former on the bottom of the kiln. Fire slow.
-
Pat Reynolds
- Posts: 6
- Joined: Mon May 28, 2012 12:23 am
Re: Flower former too high for kiln?
Thank you, Valerie. Great idea.
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Flower former too high for kiln?
Make sure your kiln floor is well kiln washed.