Has anyone used one of these??

http://www.misterart.com/crafts/stencil ... g-kit.html
comments? something better? :-k

thanks,
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: stencil cutter

Post by Brad Walker »

I've used a different brand, but it looks similar. Works very well for cutting contact paper or thin vinyl resist.
tbach
Posts: 33
Joined: Tue Jan 04, 2011 11:35 pm
Location: Hillsboro, Oregon

Re: stencil cutter

Post by tbach »

Yes I have, and it works very well. For me, it was a lot cleaner cut than I got using xacto knife. It was also a lot faster.
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: stencil cutter

Post by Don Burt »

I use one. I stencil for airbrush mostly. I replace the cutting tip with a small brass round head bolt and use it to hold a sewing needle. I run it through a soldering iron temperature control at about half power that it doesn't overheat the needle and cause it to quickly lose temper. Even so, I replace the sewing needles after a few minutes of cutting because a sharp point makes for the most precise cut.
Cynthia O
Posts: 12
Joined: Fri Nov 05, 2004 2:36 pm
Location: Salt Lake City, Utah

Re: stencil cutter

Post by Cynthia O »

Buy extra tips (or use Don's trick). I don't have a resistor, so my iron is always on full heat. Anyway...I use a hone (those diamond plated hones you can get from Harbor Freight) and resharpen the tips as they dull.
http://www.harborfreight.com/3-piece-2- ... 36799.html

I've only used this tool for cutting thin resist. An exacto is better for thicker resist or buttercut.
Image
http://cynthiaoliver.blogspot.com/

"A happy childhood has spoiled many a promising life."
Robertson Davies
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: stencil cutter

Post by Laurie Spray »

thanks everyone!!!
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Post Reply