				use of diamond hand pad
				Posted: Tue Feb 03, 2004 10:32 am
				by Marilyn Kaminski
				I have a couple pieces with a burr on the edge -- a little sharp bit that's very unappealing.  Small enough that it seems a waste to grind and go through a whole fire-polishing cycle ... is this something that a diamond hand pad would clean up?
Thanks -- Marilyn
			 
			
					
				
				Posted: Tue Feb 03, 2004 10:44 am
				by Ron Coleman
				The diamond pads will work, but I find them hard to control on small edges.  One slip and you scratch the surface of your piece.
For fine details I like to use diamond honing sticks.
http://shop.woodcraft.com/Woodcraft/pro ... D4637914AA
Ron
 
			
					
				
				Posted: Tue Feb 03, 2004 10:50 am
				by Marilyn Kaminski
				Coarse, medium, fine, or superfine?
- M
			 
			
					
				
				Posted: Tue Feb 03, 2004 10:56 am
				by Ron Coleman
				Marilyn Kaminski wrote:Coarse, medium, fine, or superfine?
- M
I find the fine and superfine to be the most useful.