how to remove silicone glue?
Moderators: Brad Walker, Tony Smith
how to remove silicone glue?
I used some silicone glue, it did the trick, and now I want to remove it, completely. Suggestions? It's been on the piece for about a month.
-
Nicole Hanna
- Posts: 27
- Joined: Wed Jul 27, 2005 10:17 am
- Location: SW Missouri
- Contact:
Re: how to remove silicone glue?
Razor blade works if you can get it behind the glue. I think some chemical dissolves it but can't remember what it is....acetone? mineral spirits? My husband is gone and not answering his phone!
N.
N.
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: how to remove silicone glue?
You want to get as much as possible off with the razor blade, and your thumb, then clean up the residue with acetone.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
Re: how to remove silicone glue?
The only way I found to successfully remove silicone from glass is to put the glass in the kiln and take it to 800.
Greg
Re: how to remove silicone glue?
There is a commercial Silicone solvent. Nasty stuff.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: how to remove silicone glue?
mek works. also nasty. rosanna
artist, owner of wanchese art studio, marine finisher
Re: how to remove silicone glue?
I have successfully used razor blades and thumb nails but find that I often want to make it pretty by using 0000 steel wool with some whiting. The whiting helps stop the silicone from re-sticking and the steel wool, as much as I don't like using it, is fairly gentle as it removes more & more silicone, with little more whiting and some elbow grease. - Tod
please visit Beall Glass Studio on Face Book
Re: how to remove silicone glue?
Paint thinner works on E6000. Might try it on silicone.
Take care.
Dawn
Dawn
-
Georgia Novak
- Posts: 28
- Joined: Wed Jun 04, 2003 2:54 am
Re: how to remove silicone glue?
Many years ago when I first started stained glass, I glued a panel into the grooved out area of a wooden door, per instructions of teacher. Well, or course a piece broke and the panel had to be removed. I wrote to e-6000 and asked how. They sent me a list in order from weak to strong. I think I finally ended up using turpentine which was the strongest on the list. It took a while but finally gave. Sorry for the shaggy dog story. Georgia