Does anyone have any experience of using iridised glass (uncapped) for tiles that are going to be submerged in a swimming pool? Just wondering if the coating will stand up to the chemicals in the water?
Thanks
Becky
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Bullseye Iridised coating

Post by jim burchett »

Yes
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
becky wills
Posts: 7
Joined: Sat Feb 19, 2005 6:19 pm
Location: Bristol, UK
Contact:

Re: Bullseye Iridised coating

Post by becky wills »

Thanks :)) Nice succinct answer!
Terry Curtis
Posts: 15
Joined: Tue Apr 04, 2006 9:26 pm
Location: Goffstown, NH
Contact:

Re: Bullseye Iridised coating

Post by Terry Curtis »

I'm curious Jim. Was the Yes in response to the frst or second question or to both?
Terry Curtis
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Bullseye Iridised coating

Post by Bert Weiss »

Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
becky wills
Posts: 7
Joined: Sat Feb 19, 2005 6:19 pm
Location: Bristol, UK
Contact:

Re: Bullseye Iridised coating

Post by becky wills »

Beautiful pool...
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Bullseye Iridised coating

Post by Morganica »

Wow. That is gorgeous. I want a bathtub like that!
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Bullseye Iridised coating

Post by Bert Weiss »

Morganica wrote:Wow. That is gorgeous. I want a bathtub like that!
Yeah!

A lot of their tiles are Bullseye irrids fired irrid side down, and the tiles become reversible. The irrid side resists picking up texture so they look really nice. Compared to dichro, these tiles have a some pop, at a much lower cost.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions