resist print question

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
deerick
Posts: 11
Joined: Wed Mar 17, 2010 9:52 pm

resist print question

Post by deerick »

Hi - I just read Jody Walker book and want to try resist print meathod. Can I put the painted resist glass right on to a swirl bottom piece and full fuse all at one time? Or do I have to tack fuse the painted resist glass first then full fuse it on to another piece? also, do you have to clear cap the painted piece? Thank you
Diane
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: resist print question

Post by Brad Walker »

You can full fuse in one firing if you like. Just make sure the enamel is dry before firing.

You don't have to clear cap.