flattening a bowl
Moderators: Brad Walker, Tony Smith
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
flattening a bowl
Have a bowl that I foolishly tried slump and firepolish at the same time..now the exterior of the bowl picked up some marks where it hung up on the mold. I would like to re flatten the bowl and am wondering if it would be better to have it rightside up or upside down to successfully reflatten it? any thoughts? Thanks.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Re: flattening a bowl
Right side up. Upside down risks trapping air.
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: flattening a bowl
Thanks brock
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie