Page 1 of 1
husqvarna vs mk?
Posted: Wed Aug 29, 2012 11:50 am
by Redfisher
I need to purchase a better 10" diamond blade. I looked for the answer with no luck.
Which is better?? Is there another brand that's better?? What do you use?
Thanks in advance!!
Re: husqvarna vs mk?
Posted: Wed Aug 29, 2012 12:22 pm
by Marty
what are you cutting?
Re: husqvarna vs mk?
Posted: Wed Aug 29, 2012 1:31 pm
by Valerie Adams
Talk to the folks at His Glassworks, linked above in the board sponsors.
Re: husqvarna vs mk?
Posted: Wed Aug 29, 2012 5:06 pm
by Redfisher
Marty...mostly cutting tops off of dropped pieces and pattern bars.
Thanks Valerie!
Re: husqvarna vs mk?
Posted: Wed Aug 29, 2012 7:00 pm
by Marty
I really really like HIS's Result blade- get the thicker (.040) one and be nice to it (no constant dressing!).
Re: husqvarna vs mk?
Posted: Fri Aug 31, 2012 1:26 pm
by Redfisher
I'll check out Hus! Thanks Marty!