Page 1 of 1

Cutting glass 45 angle

Posted: Wed Sep 05, 2012 8:13 am
by osnat
Hello,

What is the way to cut the 3 mm side of the glass in 45 angle.

I hope my q.is clear. I doing a glass strip work,and a design includ kind of triangle.
Thank
Osnat

Re: Cutting glass 45 angle

Posted: Wed Sep 05, 2012 4:44 pm
by Stephen Richard
An angle jig on a flat lap

Re: Cutting glass 45 angle

Posted: Fri Sep 07, 2012 8:07 am
by Dairy Queen
281377_1890417661503_2778352_n.jpg

Re: Cutting glass 45 angle

Posted: Fri Sep 07, 2012 8:09 am
by Dairy Queen
The radial arm tile saw posted above can be set at specific angles. Cost about $200-250 at Lowe's.

Re: Cutting glass 45 angle

Posted: Tue Sep 11, 2012 5:26 pm
by Havi
OSNAT,
I think that if you can, you'd better fuse the glass strips first, and then cut it with a saw in an angle.
[as opposed to cut separately each glass strip]

Good luck,
Havi

Re: Cutting glass 45 angle

Posted: Wed Sep 12, 2012 12:42 pm
by osnat
Thanks evryone.

Osnat