I have lost my notes for firing Effetre soft glass.
I would like to try something with rods and murrini, but do not remember the full fuse temp, or best annealing tempurature.
Has anyone here done fusing with this mainly bead making glass?
Do you have fusing and annealing temps for 104 coe
Moderators: Brad Walker, Tony Smith
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Do you have fusing and annealing temps for 104 coe
Here is a table from Kirwan that might be useful
http://glasstips.blogspot.co.uk/2010/07 ... fetre.html
http://glasstips.blogspot.co.uk/2010/07 ... fetre.html