I searched "kilnwash stainless steel" and did not find the information I am seeking however, I did discover that I should not have purchased ceramic floral formers....  Never really was interested in making these but have a request and realize they sell out at the local glass store!
   If I do not have an airbrush set up, what is the best way to kilnwash stainless steel?  Do I heat it in the oven or with a hairdryer first and use a brush?
Chelsea
			
			
									
						
										
						kilnwashing stainless steel floral formers
Moderator: Tony Smith
- 
				Chelseaglass
- Posts: 23
- Joined: Sat Jul 18, 2009 10:10 pm
Re: kilnwashing stainless steel floral formers
Heat it in your kiln to 550-turn off kiln, pull the  hot mold out carefully with  pliers. Lay  it  on a drop cloth that won't  burn or melt to catch overspray.  a couple wood or kiln brick bits will raise  the  mold off the surface.  Spray on Bullseye kilnwash with   a hand held  spray  bottle with a fine  mist. Practice  first-  you  only have a few seconds before the mold cools. It will spit and steam but it cools down after  2 or  3 three spritzes.   Put it back in the kiln  and reheat  back up to 550.  Repeat this  4 or 5 times.  If you spray  too much too fast,  the kilnwash  just runs off and leaves  bare spots that will stick to the glass and  make cracks. Then you have to carefully respray that area. Another  helper to  raise and lower the  kiln  lid is welcome.  A brush is too coarse. Or-  they  say  boron  nitride  is  a good separator, too.  There must be  more info in the  archives on this.
			
			
									
						
										
						- 
				bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: kilnwashing stainless steel floral formers
I first sandblast then use a hand held plumbers torch to heat the mold, apply wash and reheat till dry. Repeat 4 times, you mold is ready in about 5 minutes.
Bob
			
			
									
						
										
						Bob
- 
				rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: kilnwashing stainless steel floral formers
i use a heat gun to heat and spray with a critter brand spray gun. rosanna
			
			
									
						
							artist, owner of wanchese art studio, marine finisher
			
						- 
				Chelseaglass
- Posts: 23
- Joined: Sat Jul 18, 2009 10:10 pm
Re: kilnwashing stainless steel floral formers
Thank you for the information.  I have a hot head torch set up and never thought of using it to heat the form.
			
			
									
						
										
						Re: kilnwashing stainless steel floral formers
Torch on it!  Great Idea!
			
			
									
						
										
						Re: kilnwashing stainless steel floral formers
I use methyl hydrate and kiln wash. Coat the mold, place it on a kiln shelf. Close all containers of methyl hydrate ( very flammable fumes) Light the form from the bottom and watch it dry instantly. Don't touch again or you will remove the perfectly smooth application of wash. I use Bullseye Pink Wash, love the stuff.
I know some will say this is dangerous, but so is taking a hot mold out of kiln. OUCH. Stainless is hot. PLUS this method satifies my pyro needs. I also blow glass so hot is fun. Just be safe about this and it works great.Lia
			
			
									
						
										
						I know some will say this is dangerous, but so is taking a hot mold out of kiln. OUCH. Stainless is hot. PLUS this method satifies my pyro needs. I also blow glass so hot is fun. Just be safe about this and it works great.Lia