Page 1 of 1

removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 11:36 am
by Carol Ann
I slumped over a stainless mold with too hot a temperature. Some of the glass is baked on. Is there way to remove the stuck glass from the stainless mold?
Thanks in advance,
Carol Ann

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 11:42 am
by rosanna gusler
get it hot and dump into water. rosanna

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 11:56 am
by Carol Ann
thanks Rosanna I will give it a try.

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 12:40 pm
by rosanna gusler
use eye protection. rosanna.

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 12:42 pm
by Havi
Rosanna,
Will it not explode? or this is the reason for the safety glasses?


thanks,

Havi

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 1:36 pm
by rosanna gusler
it might pop and steam but not explode. safety glasses are cheap and easy insurance. i got a piece of glass in my eye a couple of weeks ago doing something stupid. i was lucky. i washed it out with no harm. safty glasses or a face shield thet took all of 2 seconds to put on would have saved me alot of angst. rosanna

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 2:53 pm
by Havi
glad to hear you are OK now!






havi

Re: removing glass from stainless steel mold

Posted: Wed Sep 19, 2012 5:40 pm
by Carol Ann
Thanks Havi and Rosanna,
I will wear safety glasses and face shield. Thanks for the information