Hi,
I want to make some glass nuggets from the scrap Sys 96 glass I have, I will be cutting it into 1/2" squares and fusing 2 squares together. I have never made them before and I have a new kiln it's a Paragon Fusion 8 with sentry controller. Can someone please give me a firing schedule that I could start off with, I am still trying to get used to this new kiln.
Thank you
Schedule needed for glass nuggets
Moderators: Brad Walker, Tony Smith
Re: Schedule needed for glass nuggets
Turn it on high until done.
Turn it off.
Turn it off.
Re: Schedule needed for glass nuggets
So in other words do I ramp up ASAP to around 1450 check and then turn off?
Re: Schedule needed for glass nuggets
Yeah, that's all there is to it.Vicki M wrote:So in other words do I ramp up ASAP to around 1450 check and then turn off?
-
- Posts: 307
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: Schedule needed for glass nuggets
Vicki,
You may need to hold some at 1450.
Check to see if they are done, then turn off the kiln.
Barry
You may need to hold some at 1450.
Check to see if they are done, then turn off the kiln.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
Re: Schedule needed for glass nuggets
"I want to make some glass nuggets . . ."
"Turn it on high until done. Turn it off."
"So in other words do I ramp up ASAP to around 1450 check and then turn off?"
Get it Barry? . . . until done . . . check . . .
"Turn it on high until done. Turn it off."
"So in other words do I ramp up ASAP to around 1450 check and then turn off?"
Get it Barry? . . . until done . . . check . . .
-
- Posts: 58
- Joined: Sat Jul 30, 2005 6:25 pm
- Location: Portland OR
- Contact:
Re: Schedule needed for glass nuggets
We need a "Like" button on this board.
Re: Schedule needed for glass nuggets
Thanks so much everyone as they say you don't learn if you don't ask. Even for the simplest of things. Thank you again for taking the time to reply.