George's Rigidizer

Posted: Wed Nov 14, 2012 2:57 pm
by dkingman
Has anyone used George's Rigidizer? It is a blue-green liquid. I coated 1/8 inch fiber with it but noticed the back was still white. Should I coat the back as well? There was no instructions for pre-firing it.

Thanks,

Dave

Re: George's Rigidizer

Posted: Wed Nov 14, 2012 5:49 pm
by rosanna gusler
i would coat both sides. Fire to whatever temp you are going to use it at kiln wash and use .rosannat

Re: George's Rigidizer

Posted: Thu Nov 15, 2012 6:17 pm
by dkingman
Thanks Rosanna