Drilling in Bisque

Posted: Fri Nov 30, 2012 1:07 pm
by RachelM
Hi All:

I have a friend who "came into" a bunch of bisque molds. She says I can take a few for my glass fusion works.
She has a few plates and bowls that I am interested in.

But, no holes, which I know I need, to release air pockets and not have my glass bubble up.

Thoughts on how to drill holes....types of drill bits, do I need to drill wet or dry, etc. :?:

Thanks!

Rachel :D
imaglassydiva@aol.com

Re: Drilling in Bisque

Posted: Fri Nov 30, 2012 1:18 pm
by Laurie Spray
If they are shallow try them without holes.......no need
If they are deeper and you feel you have to drill them i just use a dremmel with a diamond rough with water but.......get thru the clay and them reem it to the size you want.....not very big. When you use kiln was be sure it does not clog up your holes.

Re: Drilling in Bisque

Posted: Fri Nov 30, 2012 1:42 pm
by Bert Weiss
If you look in the drill bit section of a hardware store, you will find several different types of bits recommended for ceramic drilling. Just like with glass, the hard part is breaking through the second surface. So, be sure to start your hole from the inside of the bowl, assuming you are slumping in. Be aware that a hole itself is not enough, The hole has to have a pathway out to open air. If the bowl is footed you will have to prop it up in such a way as to open up that path. Also remember to unclog the hole after you kilnwash the bowl.

Re: Drilling in Bisque

Posted: Fri Nov 30, 2012 3:02 pm
by Brock
If the mold is flat then you will have to raise it to ensure air can escape via the drilled holes .
If the mold is footed, then no problem, just drill and slump.

Re: Drilling in Bisque

Posted: Fri Nov 30, 2012 6:27 pm
by Morganica
If it's bisqueware, you can usually take a sharp nail or screw and gently dig out a small starter hole, which will help keep the bit from skittering all over the surface. Bisque has a matte surface anyway, so it's easier to drill that fully fired/glazed ceramics. Give yourself plenty of elbow room, then set the point of the bit in the starter hole, at an angle of maybe 30 degrees off the surface. Start the drill as slowly as possible, and raise the drill as it begins to bite into the ceramic, until it's perpendicular to the surface. Once the drill is well-settled in the hole, speed it up a bit. Be patient, don't press down hard on the drill but allow it to grind out the material.

However, I agree with Laurie--there's not much point in drilling holes until you know you need them. You've also got to remember that there's got to be a good airflow around those holes, so if you drill through the bottom of the piece it will need to be elevated to work.

Ooops...sorry, Brock, didn't see your post. Yeah. What he said. ;-)

Re: Drilling in Bisque

Posted: Fri Nov 30, 2012 11:57 pm
by RachelM
Thank you ALL!

Rachel