Spray A separated, how to fix?

Post by Jodi Longobardo »

I have had a bottle of Spray A for a few years--I never get devit now that I stopped fire polishing on thinfire, so I have never used it. Recently I took a class where we were told that we should use Spray A when doing a certain technique because dark colors had a tendency to devit, so I wanted to go ahead and use it. However, I discovered that it had separated into a milky liquid and a hard white solid. I tried shaking it, but it didn't cause the solid to go back into solution. Any suggestions on how to fix this, or should I just buy a new bottle which will also languish in a drawer except when doing this technique? Thanks in advance for any advice!

--jodi
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Spray A separated, how to fix?

Post by Stephen Richard »

It requires an extraordinary amount of shaking and agitation to get it mixed again, but it is possible.
Alternatives are saturated solution of borax or sprinkled clear powder or fine clear frit over the top of the piece.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Spray A separated, how to fix?

Post by Laurie Spray »

I keep marbles in my jar of spray a.....lots of marbles.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Spray A separated, how to fix?

Post by Morganica »

Put it into a (microwave-safe) container you don't care about, stick it in the microwave and heat it to a simmer (not to a full boil). That should help it go back into solution, especially if you add marbles. ;-)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Jodi Longobardo
Posts: 34
Joined: Sat Sep 30, 2006 7:51 pm
Location: NJ

Re: Spray A separated, how to fix?

Post by Jodi Longobardo »

Aha! I was wondering if I could put it in the microwave--that's what I do with my kiln wash when it separates. Thanks everyone for the advice!

--jodi
Lynn Perry
Posts: 129
Joined: Sun Jun 08, 2003 5:27 pm
Location: East Tennessee

Re: Spray A separated, how to fix?

Post by Lynn Perry »

Morganica wrote:Put it into a (microwave-safe) container you don't care about, stick it in the microwave and heat it to a simmer (not to a full boil). That should help it go back into solution, especially if you add marbles. ;-)
Are you sure you want to heat a solvent in an appliance which can ignite the vapors?