Do I need to adjust my firing schedule when stacking shelves
Moderators: Brad Walker, Tony Smith
Do I need to adjust my firing schedule when stacking shelves
I am loading my Paragon GL24 kiln (front load, top and side elements) with many (16) smallish open face pate de verre pieces. I am thinking of adding an additional shelf with a few more pieces. I'll check on how it all looks when at the process temp, but just wondering if I should adjust the schedule ahead of time. In general, does adding another shelf affect firing schedules?
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Do I need to adjust my firing schedule when stacking she
oh yes. especially with top elements. side fire pottery kilns are fairly easy to manage with multi shelves but with a top element in play i would say no if you need the same amount of heat work on both shelves. rosanna
artist, owner of wanchese art studio, marine finisher
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Do I need to adjust my firing schedule when stacking she
I stack in my GL24. Just turn the top elements off and slow way down so that the heat reaches everything evenly. I've found that it works best with at least 6 inches between shelves. Tim
Tim Yardic
Yardic Glassworks