Post by Don Burt »

For those of us who keep an eye on ceramics decoration techniques, here's a link to look at.
Johanna De Maine
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Surface Decoration

Post by Bert Weiss »

The techniques she uses on her glazed porcelain, can all be done on any glass we might be using, with the same lustres and onglaze colors she uses. (with the possible exception of raised enamels which would need to be tested for compatibility)