I recently purchased the infinity series (texture plate and wave form slumping mold) from fuse master. There is only one hole at the bottom of the bowl form. Does it need more holes? Has anyone used this/drilled holes. Any tips?
Chris
Fuse Master Wave form slumping mold - more holes?
Moderators: Brad Walker, Tony Smith
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Fuse Master Wave form slumping mold - more holes?
You should be fine with the one hole, if it needed more holes they would of added them.
Bob
Bob