Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Keeping the drains clear

Post by Dolores »

Hello all,

I'm currently revamping my glass studio and need to install some sort of trap on my drain to prevent glass powder from clogging my sewer line. What contraption and/or device and/or brand do you all use? Is it an easy DIY? Thanks in advance!

DOLORES
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Keeping the drains clear

Post by Kevin Midgley »

A restaurant grease trap or two of them may be simplest.
GuyKass
Posts: 75
Joined: Tue Jul 15, 2008 9:53 pm

Re: Keeping the drains clear

Post by GuyKass »

This is about as simple as it gets...

I think Cynthia Morgan posted about it ages ago.

http://www.artmolds.com/product_details ... ter%20Trap

You can also do a Google search "artist sink trap"and a bunch of DIY stuff comes up for pottery studios, which look pretty simple, cheap and straight forward.
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Keeping the drains clear

Post by Tony Smith »

Agreed. The Gleco Trap is the way to go.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Re: Keeping the drains clear

Post by Dolores »

Thanks everyone! The Gleco trap looks like it will do the trick.

DOLORES
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Keeping the drains clear

Post by Morganica »

Yup, the Gleco works beautifully and it's relatively easy to buy and install. The only difficulty I've found is making sure there's sufficient space for it under the sink. Also, you've got to be sure to check it as often as the manufacturer recommends--when it fills up, it's useless, but you (or at least me) will continue using it as if it's working...
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Keeping the drains clear

Post by Barry Kaiser »

I've got a Gleco and it is easy to install. After cleaning it out the first time, I realized how much good it really does. The swarf packs like concrete. It can really do a number on your plumbing.

Barry
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Keeping the drains clear

Post by Brad Walker »

Morganica wrote:The only difficulty I've found is making sure there's sufficient space for it under the sink.
There are four different sizes. You can measure the distance from the trap to the floor to find the right one for your sink.
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Re: Keeping the drains clear

Post by Dolores »

I ordered the Gleco for my studio redo. I learned from the sediment in my Revolution saw tray just how rock-like that swarf can get and didn't want to repeat the experience in my new sewer line!