I just finished the remaking of a piece that I made last month. The initial piece had BE013 which developed stress after a number of firings. This piece has had 8 firings without stress, and without any BE013. The first one became a giveaway, and 5lbs. of BE013 became a throwaway. Live and learn.
Re: Remake frit painting
Posted: Sat Mar 02, 2013 11:29 pm
by JestersBaubles
Wow -- beautiful. I love the reflection in the water.
Dana W.
Re: Remake frit painting
Posted: Sun Mar 03, 2013 12:01 am
by Labrador
Just love it

You sure master this composition
Thank you for sharing
Sophie

Re: Remake frit painting
Posted: Sun Mar 03, 2013 2:54 pm
by Jane Morgan
Wow, stunning!
Re: Remake frit painting
Posted: Sun Mar 03, 2013 9:05 pm
by Babette (Shawn)
Nice piece David! I also dumped all of my BE0013 powder.
Re: Remake frit painting
Posted: Mon Mar 04, 2013 4:26 pm
by Risa
I was at Art Palm Beach last month...and believe I saw some of your work. Captivating and sensuous use of light and shadow. Very, very well done.
Re: Remake frit painting
Posted: Mon Mar 04, 2013 5:41 pm
by jim burchett
lovely piece
Re: Remake frit painting
Posted: Mon Mar 04, 2013 5:50 pm
by david n
Thanks for the comments, I appreciate it. It's validating to get encouragement from the glass community. Risa, my work was at Art Palm Beach last month with my gallery (unfortunately I wasn't there). They sold a large piece to someone they called a "major collector", whatever that means. It can't hurt.
Re: Remake frit painting
Posted: Tue Mar 05, 2013 11:58 am
by Zane
Very lovely piece!
Re: Remake frit painting
Posted: Tue Mar 05, 2013 8:18 pm
by glass-lady
Fantastic.
Re: Remake frit painting
Posted: Thu Mar 14, 2013 12:27 am
by Celene
Wow! That is gorgeous! That is what I'm aspiring to.

Ohhh....One day I hope...
Re: Remake frit painting
Posted: Fri Mar 15, 2013 1:11 pm
by Delberta D
This is what I would love to learn to do. I have used Michael Dupilles technique but I want my picture to have NO bubbles....I did oil painting many years back and love these results in glass. Your piece is beautiful.
Re: Remake frit painting
Posted: Sat Jun 08, 2013 9:41 am
by Andrea R
david n wrote:I just finished the remaking of a piece that I made last month. The initial piece had BE013 which developed stress after a number of firings. This piece has had 8 firings without stress, and without any BE013. The first one became a giveaway, and 5lbs. of BE013 became a throwaway. Live and learn.
What did you use in place of BE013? That opaque white?
Re: Remake frit painting
Posted: Sat Jun 08, 2013 10:13 am
by jim burchett
Wonderful piece. Anyone else looking to dump their 0013..you can dump it my way.

Re: Remake frit painting
Posted: Sat Jun 08, 2013 3:43 pm
by Havi
Very nice indeed.
May I ask what are you using instead of BE0013?
I am curiuos, have you or anybody else incurred problems with BE0013 in other forms? like sheets, or big frit? [03]
Thanks,
Havi
Re: Remake frit painting
Posted: Sun Jun 09, 2013 5:12 pm
by david n
I replaced the BE013 with BE113 (white opal) and it worked fine. I like the BE243 for snow, but it can't withstand the vitrograph temp. it turns partially clear. BTW I just returned from The Glass Weekend at Wheaton Arts in NJ today. My gallery sold this piece Sat. It was an amazing experience with demos and lectures from well-known glass artists (many collectors there too). It's held every other year. I would recommend it to anyone who loves glass.
Re: Remake frit painting
Posted: Wed Apr 30, 2014 7:11 am
by oatkaglass
Beautiful work David....haven't heard from you in awhile but it looks like you have been busy.
For anyone looking to take a class in this technique, Miriam di Fiore teaches her technique in her studio in Italy and also at various studios in the US. We are hoping to have her back teaching in our studio, Oatka School of Glass, in November 2014......

- In The Depth of Winter - Miriam di Fiore
Re: Remake frit painting
Posted: Wed Apr 30, 2014 10:01 am
by Zane
Gorgeous!
Re: Remake frit painting
Posted: Mon May 05, 2014 1:47 pm
by Linda Gilpin
Beautiful work David!! Have you used the new Warm White instead of the BE13? Any problems, or would it dull it down a touch? Thoughts?
Re: Remake frit painting
Posted: Mon May 05, 2014 8:31 pm
by twin vision glass
Oh so very beautiful!!!!!!!!! Les