I would be very grateful if someone would tell me the melting or fusing temperature of BE powder tekta 1101 and/ or clear transparent powder 1401.

Additionally, I would be grateful to know the melting / fusing temperature of fine frit 01 grind again, of tekta BE1101 and / or clear transparent 1401.


I need to know this in order to know how high. Do I need to get if I cap a piece with powder or fine frit.


Many thanks in advance

HAvi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Melting temperature

Post by Brad Walker »

Depends on the kiln and the rate at which you fire. Somewhere between 1400 and 1500F. The larger particles will take a higher temperature.

We generally fire to a full fuse when we do this, haven't experimented with how low you can get away with.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Melting temperature

Post by Havi »

Thanks, Brad




HAVI
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Melting temperature

Post by twin vision glass »

Image
Image
I am also with Brad on this one. Test it is probably the best advice I could give. My schedules have to take in flat glass, frit of all sizes , and all sorts of things happening. I go up 50 degrees per hour to 1230 and hold 2 hours, and only up to 1480. So there is my schedule and temp for powder to #3 frit size in large pieces. Les
Image
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Melting temperature

Post by Havi »

Thanks, Les,
That is a very good information, and a very interesting process