All things considered, this is a pretty good idea for most of us to read...
http://www.bullseyeglass.com/images/sto ... tes_03.pdf
Seriously worth reading... Bullseye
Moderators: Brad Walker, Tony Smith
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Seriously worth reading... Bullseye
Maybe even read a few times all the pages in Stone's Firing schedules for glass for even more understanding.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Seriously worth reading... Bullseye
One of my pet peeves, Bullseye is also guilty of this .
ALL GLASS is "fuseable" But NOT compatible.
When a manufacturer says that their glass is "fusable" they are implying that it is compatible.
This has led to some very serious musunderstandings.
Rant over :>)
The other Jim
ALL GLASS is "fuseable" But NOT compatible.
When a manufacturer says that their glass is "fusable" they are implying that it is compatible.
This has led to some very serious musunderstandings.
Rant over :>)
The other Jim
Re: Seriously worth reading... Bullseye
Stone's Firing Schedules is available from Warmglass.comhttp://www.warmglass.org/servlet/the-15 ... ass/Detail and well worth twice the price (glad I bought mine before that comment!)Kevin Midgley wrote:Maybe even read a few times all the pages in Stone's Firing schedules for glass for even more understanding.
Jerry