Post by Al Bray »

Just a few pictures of my first attempt at slumping a project into deeper molds on my own.

The vessel itself is approximately 12.75" in diameter and 6.75" deep.

- Al
Attachments
0001.jpg
0002.jpg
11.jpg
Terry Curtis
Posts: 15
Joined: Tue Apr 04, 2006 9:26 pm
Location: Goffstown, NH
Contact:

Re: Deeper Slumping

Post by Terry Curtis »

Al, is this just the 2nd slump? I really like it
Terry Curtis
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Deeper Slumping

Post by bob proulx »

Nice job Al, it looks like the new kiln is working out.
Bob
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Deeper Slumping

Post by AndyT »

Beautiful!!
Barb R
Posts: 58
Joined: Tue Jul 26, 2005 3:02 pm
Location: Ft. Collins, CO

Re: Deeper Slumping

Post by Barb R »

Love it! It's gorgeous.
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Deeper Slumping

Post by Warren Weiss »

Superb!
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Deeper Slumping

Post by Morganica »

Love (adore, really) that bowl...but it's the pyramid that keeps catching my eye!
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Deeper Slumping

Post by Havi »

This is really very nice. I like the design, as well as the form.
Did you use Karl Harron's technique ?



Thanks

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Deeper Slumping

Post by twin vision glass »

I am loving what you are creating. I love also to work with reactions in the glass, and you have created a wonderful piece . I think your kiln is perfect for this. Front loading kilns can be alittle tricky for colour bar techniques as you build the piece and then lift over to the kiln , so I LOVE to drop it down , instead of try to balance it in , and this looks perfect for what I love to do. AND I toooooo love the pyramid. I like also to use sections of the bars and slice and shape. Or perhaps this is the diamond mold from Bullseye. Does not matter what mold or technique, I love it.
Leslie
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Studiodunn
Posts: 106
Joined: Sun Sep 11, 2011 9:30 am
Location: The Dunn-Inn
Contact:

Re: Deeper Slumping

Post by Studiodunn »

So Love!
“I would rather die than hate you.”
- Martin Luther King
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Deeper Slumping

Post by JestersBaubles »

Beautiful!

I want to be like all you guys when I grow up :).

Dana W
Babette (Shawn)
Posts: 103
Joined: Fri Feb 05, 2010 4:11 pm
Location: Chico California
Contact:

Re: Deeper Slumping

Post by Babette (Shawn) »

Gorgeous bowl Al! And I love your photography! The first photo with the circular shadows is very artistic...man of many talents!
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Al Bray
Posts: 42
Joined: Thu May 01, 2003 8:37 pm
Location: Lansing, Michigan
Contact:

Re: Deeper Slumping

Post by Al Bray »

Thank you to everyone for taking the time to provide feedback.

To answer the questions:

Havi, I did use the first two molds from the 3 mold set that are used in Karl’s Perfect Vessel workshops for slumping this project.

Terry, I decided not to do the third slump on this particular project because I wanted a wider flared out bell top rim to play with when flatlapping. I felt that was necessary so that the eye easily flowed over the rim from the design on the inside to the center design element going on with the outside. In my thinking, the steeper walls would have made that transition much more definite and resulted in them “feeling” more disconnected.

Morganica and Leslie, the pyramid actually came about as a way for repurposing the scrap that results from the construction of the main project, as well as cut down on all the excess space that scrap takes up in my small studio space trying to store it for that “future” project.

The boarder glass from cutting the circle blanks is tile nipped up into smaller pieces and the excess frits/powders (that fall off or purposefully brushed off) are gathered up and used in these rather than placing it all back in their original container risking cross contamination.

Sometimes you can see the order in which the main project was constructed in the layering and it relates back to the main project. Sometimes not so much.

The mold used for this one was from a set of stainless steel jello molds that I picked up in cooking store. I very recently purchased the larger Bullseye pyramid casting mold as I think will be much easier to deal with due to it's flat base and, being ceramic, no sprawling at the higher temps where these are fused.

Thanks again to everyone for your comments.
- Al
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Deeper Slumping

Post by Havi »

- - - -
And thank you for the detailed response and the beautiful piece!




Havi
one day I shall do one of these too [probabley not as pretty]
Last edited by Havi on Tue Mar 19, 2013 4:32 pm, edited 1 time in total.
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Raphael Schnepf
Posts: 24
Joined: Sat Oct 14, 2006 11:31 pm
Location: Milwaukie Oregon
Contact:

Re: Deeper Slumping

Post by Raphael Schnepf »

I agree with Cinthia about the pyramid. It really caught my eye.
Richard Blummer
Posts: 13
Joined: Wed Jul 14, 2010 9:15 am
Location: Egg Harbor Township, NJ
Contact:

Re: Deeper Slumping

Post by Richard Blummer »

Wow, both the pyramid and the bowl are spectacular!

=D> =D> =D>
אָשֵׁר חַיִּים
Post Reply