I've noticed that my kiln has a distinctive odor, kind of like hot bricks I guess, at a certain point in the ramp up, 800F or so. But it goes away before 1000F and doesn't recur during the rest of the cycle.
It's not surprising to me that something made of hot bricks should smell like hot bricks, but you'd think it would smell that way the whole time it was hot.
Wondering if it might be something else, like I don't know, the glue or Sharpie marks burning off. Anyone else encounter this?