I have a project where I need a few copies of a white dove fused on/between clear. The spread wings have fine details. something like this
http://4.bp.blogspot.com/-2zwNWOMnTEs/T ... e-dove.JPG
Of course I will use my own design variant.
Etching on Tekta did not have enough contrast. Sandblasting should be better.
Up to now the best rsult was cutting the dove in 2mm fiber paper, slumping Tekta over it, turning upside down and filled with white powder. That is not exactly a production method.
Any suggestions
-lauri
White decal or other images
Moderators: Brad Walker, Tony Smith
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: White decal or other images
Try making your own flashed glass, either with blue frit or blue vitreous enamel, Then sandblast through the blue. You could also screen print the white, or have custom decals made.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: White decal or other images
Bert's "make your own flash glass "suggestion would be the first choice (here.)
But that being said a simple screen printing of it would work great also. Barry Kaiser sells everything you need to do it and his support is VERY good. And considering what you are doing, you won't need to make a big $$$ investment/
Email him or go to his website.
But that being said a simple screen printing of it would work great also. Barry Kaiser sells everything you need to do it and his support is VERY good. And considering what you are doing, you won't need to make a big $$$ investment/
Email him or go to his website.
Re: White decal or other images
If you have the Bullseye video subscription, look for Stacy Smith's screen printing with powdered frit demonstrations. I don't know if that's the same as Barry's--silk screening with a mesh that admits powder, basically. It's very exact and reproducible.
You can see some of her latest work here: http://www.bullseyegallery.com/Artist-D ... istsID=403
You can see some of her latest work here: http://www.bullseyegallery.com/Artist-D ... istsID=403
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)