Have been busy fusing tiles, plates, cabs and a bowl. Some edge construction and a nice pattern bar piece, all going pretty well so far. Bowl didn't come out great but I really didn't properly true up the edges of the blank before slumping, so that was my fault. Can't expect it to magically turn round while slumping, eh?
I bought several molds, one is the large BE Square plate. However, the bottom (working side) of the mold seems slightly lumpy and not smooth like my other, smaller square molds. Is there a way to fix this? Can I (carefully) remove those high spots with the right grit emory cloth? Filter mask on of course.
Other suggestions?
Thanks
I bought several molds, one is the large BE Square plate. However, the bottom (working side) of the mold seems slightly lumpy and not smooth like my other, smaller square molds. Is there a way to fix this? Can I (carefully) remove those high spots with the right grit emory cloth? Filter mask on of course.