Page 1 of 1
New tutorial
Posted: Sat May 04, 2013 12:44 pm
by Laurie Spray
I have just completed a new tutorial on the "Pattern Bar Flow Technique". Thought I would share it here. It is too much fun! We have just barely dented the surface on the fun possibilites of this technique and I am loving it!
http://www.igrowhydro.com/fusedglassart ... hnique.pdf
Re: New tutorial
Posted: Sat May 04, 2013 1:58 pm
by Barry Kaiser
Cool look and so easy!!
Barry
Re: New tutorial
Posted: Sat May 04, 2013 3:43 pm
by Gail L
Going to try it with my 12 !/2" SS round from Laurie !
Re: New tutorial
Posted: Sat May 04, 2013 9:13 pm
by JestersBaubles
Thank you for sharing the info, Laurie. I particularly like the design of the piece in the very last picture (love the color purple).
Dana W.
Re: New tutorial
Posted: Sat May 04, 2013 9:57 pm
by Laurie Spray
These pictures are just some starters learning the weights and fusing programs. It has opened my mind to lots and lots of new possibilities! I have had a HUGE email response today from customers that are so excited! Really fun! Soon I will have all the weights calculated to make it even easier! I will add more pictures to the tutorial on our site as they come out of the kilns.

Re: New tutorial
Posted: Thu May 09, 2013 10:49 pm
by Eric Baker
Those are fun, and a lot of possibilities exist. I had a similar idea a few years back with some scrap pattern bar pieces, but never followed up--just left it sitting in the 'try it someday' pile.
Now I'll brush off the dust and go with the 'flow'.
Thanks for sharing, Laurie.
warm regards,
Eric
Re: New tutorial
Posted: Sat May 11, 2013 5:03 pm
by Laurie Spray
Here is a set of pattern bars that were made of old bullseye pattern bars that I was not crazy about. pic is of 4 sets of them after I had done the "flow" in one of our stainless steel rings. Having way to much fun here! This one sold right out of the slump still warm!
Re: New tutorial
Posted: Sun May 12, 2013 8:26 am
by JestersBaubles
Laurie Spray wrote:Here is a set of pattern bars that were made of old bullseye pattern bars that I was not crazy about. pic is of 4 sets of them after I had done the "flow" in one of our stainless steel rings. Having way to much fun here! This one sold right out of the slump still warm!
Beautiful, Laurie.
I ordered a new tile saw (MX-370exp) that should arrive early this next week. Can't wait to get cutting!
Dana W.
Re: New tutorial
Posted: Mon May 13, 2013 9:33 am
by Laurie Spray
Re: New tutorial
Posted: Mon May 13, 2013 9:33 am
by Laurie Spray
Re: New tutorial
Posted: Wed May 22, 2013 11:31 am
by Mark Wright
This is great fun!
Thanks Laurie.

Re: New tutorial
Posted: Wed May 22, 2013 11:52 am
by Eryc F.
Mark that's great!!!! Well done!
I'm going to start playing with bars over the summer.
Re: New tutorial
Posted: Wed May 22, 2013 11:59 am
by Laurie Spray
Very addictive.........so much fun to do something new!!!!