I screen printed a 3.5 x 3 piece meant to be a night light. It looks fine except the design isn't balanced. Because it's a roadrunner there's no way to cut it down to balance it without losing the tail. I have no idea why I didn't notice this before the last fuse. I just don't like it but imagine that I could use it as part of another, larger piece--e.g., a small plate. Originally, it was 3 mm clear fused ink side down over a 2 mm Bullseye base.

I would really appreciate to know if there's a way to salvage this? Many thanks,

Drewcilla

Re: Help reusing fully fused piece

Posted: Wed May 08, 2013 1:31 pm
by lorimendenhall
I have not done this yet but I think it's fine to incorporate it into a new piece and full fuse again.

Re: Help reusing fully fused piece

Posted: Wed May 08, 2013 8:38 pm
by Laurie Spray
I throw things like that in a box until I am ready to do a pot melt or a pattern bar!

Re: Help reusing fully fused piece

Posted: Fri May 10, 2013 1:02 pm
by desjo
Laurie Spray wrote:I throw things like that in a box until I am ready to do a pot melt or a pattern bar!
I'm with Laurie. That's what I do with my "Hall of Shame" items and it makes for some interesting results.