Help reusing fully fused piece
Posted: Wed May 08, 2013 12:44 pm
I screen printed a 3.5 x 3 piece meant to be a night light. It looks fine except the design isn't balanced. Because it's a roadrunner there's no way to cut it down to balance it without losing the tail. I have no idea why I didn't notice this before the last fuse. I just don't like it but imagine that I could use it as part of another, larger piece--e.g., a small plate. Originally, it was 3 mm clear fused ink side down over a 2 mm Bullseye base.
I would really appreciate to know if there's a way to salvage this? Many thanks,
Drewcilla
I would really appreciate to know if there's a way to salvage this? Many thanks,
Drewcilla