ceramiguard draping Q?
Posted: Tue Feb 10, 2004 9:49 am
				
				i want to use a square of ceramiguard to drape a circle over to make a square table top with turned down edges. should i put a thick piece of fiber paper (1/4") on top and extending out past the edges just a little as a buffer? i am afraid that the glass will  grab the ceramiguard on cool down otherwise. i have done plenty of drops through but never a drape over. and while we are on the subject, how about rigidized fiber? does it  get grabbed on cool down?  i just do not want to take the time to finish dressing my steel plates today. rosanna