Uroborus Ring Mottle at Painting Temps?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Uroborus Ring Mottle at Painting Temps?

Post by Buttercup »

On this old thread:
http://www.warmglass.com/phpBB/viewtopi ... e&start=20

it seems that ring mottles lose their distinctive pattern at fusing temps. Can anyone tell me if they will stand painting and firing temps, please, without losing the mottles? I have a tiny amount and don't want to experiment with it if someone knows the answer already. Thanks for any input. Jen

EDIT. Just found out that it can't be done. Damn! :cry: