I'm trying to tack fuse two fused pieces 3X2" into an L shape to use as a simple candle holder. I'm trying to use dams today to hold it upright.
Have to wait for results tomorrow. Any ideas?
Thanks
tac fusing L shape
Moderators: Brad Walker, Tony Smith
-
Mike Byers
- Posts: 56
- Joined: Mon Mar 10, 2003 6:57 pm
- Location: west central Indiana
- Contact:
It might be easier to make an L-shape by slumping over something like a piece of angle iron. For making more than one or two, I'd cut and weld some stainless steel to the desired shape, and then give it a good coat of shelf primer. I've made light fixtures this way, and an easy way to line the piece of glass up on the slumping form is to use a felt tip marker to mark a straight line on the glass and then line this up with the form. The mark burns off when the glass is slumped, or at least it has for me.
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
l shape
ThanksMike Byers wrote:It might be easier to make an L-shape by slumping over something like a piece of angle iron. For making more than one or two, I'd cut and weld some stainless steel to the desired shape, and then give it a good coat of shelf primer. I've made light fixtures this way, and an easy way to line the piece of glass up on the slumping form is to use a felt tip marker to mark a straight line on the glass and then line this up with the form. The mark burns off when the glass is slumped, or at least it has for me.
Of course! It seems so obvious now. But for a beginner, it's all new.
Thanks so much! I'd really like to get into light fixtures too as light and glass are for me the ultimate. Do you know of any resources where I could get some ideas for some simple starter projects...ie books, sites, etc?