Page 1 of 1

Using bubble powder or metallic bubble powder

Posted: Fri Jul 26, 2013 10:22 am
by mjfglass
I was wondering about others experience using bubble powder. I got some bronze and pearl metallic bubble powder from http://www.bluedragonglass.com. The sheet of glass I made turned out pretty cool. The colors from the sheet on the bottom came through to the top, great marbling effect, cool metallic banding and a couple of spots looked almost like a geode or natural stone where the metal flakes were concentrated. Wondering how others used this product and what your results were. Here are some pics.
Image
Image
Image
Image