what's the most popular tile size?
Moderators: Brad Walker, Tony Smith
-
Kate Saunders
- Posts: 53
- Joined: Thu Mar 18, 2004 10:53 pm
what's the most popular tile size?
I'm doing the Audubon Wild Arts Festival in Portland in November, which I've been part of for quite a few years. I like to do something new every year, and this year I'm considering using photo resist technique from my own photos of birds and wolves and putting them on tiles. I make a 3.5" dish with botanical designs that's popular, but I was thinking in order to not confuse people with the same size dish with two different prices (my photo resist dishes would have to be more expensive) I'd make the bird and wolf designs into tiles. Is there a standard size for small tiles, or a size that sells the best? The tiles could always be used as coasters, but I was hoping to move them into a more upscale market. No doubt they won't sell as well as a functional dish, but I'm ready to try something new. Maybe. Thanks! Kate
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: what's the most popular tile size?
A lot of the hardware that you see for holding tiles ( for instance, boxes) are in 4 inches in 6 inch sizes.
Dana
Dana
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: what's the most popular tile size?
Tiles come in 1" x 1". 2" x 2", 4" x 4", 6" x 6", and 12' x 12", among others, including rectangular ones that fit with square ones, when you include the grout space.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: what's the most popular tile size?
That's not what she asked.
She wants to know what the MOST POPULAR one(s) are
Jim
She wants to know what the MOST POPULAR one(s) are
Jim
Bert Weiss wrote:Tiles come in 1" x 1". 2" x 2", 4" x 4", 6" x 6", and 12' x 12", among others, including rectangular ones that fit with square ones, when you include the grout space.
Re: what's the most popular tile size?
4"x4" was once the industry standard for houses (at least is seems that way in the south). I'd suggest that size, and if your customers complain, tell them to stick it.
OK, maybe customer service is not my forte.
OK, maybe customer service is not my forte.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: what's the most popular tile size?
Jim, these are all popular sizes. I thought Kate's goal was to match standard sizes, not a popularity contest. 3.5 x 3.5 is not a popular or standard size. And, BTW those measurements are not exact. I just measured a 6 x 6 in my kitchen and it is 5 7/8".jim simmons wrote:That's not what she asked.
She wants to know what the MOST POPULAR one(s) are
Jim
Bert Weiss wrote:Tiles come in 1" x 1". 2" x 2", 4" x 4", 6" x 6", and 12' x 12", among others, including rectangular ones that fit with square ones, when you include the grout space.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: what's the most popular tile size?
Bert the reason they are a little smaller is to take the spacers into consideration, that is mostly for floor tiles.
Bob
Bob
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: what's the most popular tile size?
I had to laugh. I measured the 6x6 tiles that are installed in 2 places on my kitchen walls. I thought they were 4 x 4's, but they are 6 x 6's. So I guess other tiles take the grout line in to consideration, as well.bob proulx wrote:Bert the reason they are a little smaller is to take the spacers into consideration, that is mostly for floor tiles.
Bob
BTW these 6 x 6's are white wall tiles from Home Depot. Mine have a mural painted on them using Ferro Sunshine series onglaze colors, the same ones I use for painting on fused glass. Once the paint is dry, the tiles can be fired in holders that keep them upright, so you can get a lot of them in a kiln load. Otherwise they behave much the same on tile or glass.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Kate Saunders
- Posts: 53
- Joined: Thu Mar 18, 2004 10:53 pm
Re: what's the most popular tile size?
Hmmmm.....I'm leaning towards 4 x 4 at the moment. If they don't sell as tile I'll slump them into dishes and have them another time as dishes. Ever the capitalist.
-
Kate Saunders
- Posts: 53
- Joined: Thu Mar 18, 2004 10:53 pm
Re: what's the most popular tile size?
Yes, I'll make 4 x 4's that are actually a tad bit smaller. Thanks for the information!
Re: what's the most popular tile size?
I use fused tiles in these black metal trivets purchased from Ed Hoy, and the size for a nice fit is 4 1/4" sq. People stopping by our gallery find these to be a good bargain because they actually serve a purpose - folks here are so darn practical!