Page 1 of 1

halo lustre

Posted: Fri Sep 20, 2013 8:52 pm
by Cheryl
does anyone know if there is a current supplier? I love this stuff but have had no luck finding any in the past 2 years.

Re: halo lustre

Posted: Fri Sep 20, 2013 10:14 pm
by Brad Walker
As far as I know, it's no longer being made.

When Engelhard was purchased by BASF around half a dozen years ago, the Hanovia division of Engelhard (which made the Halo lusters) was shut down. I believe Duncan still makes some of the gold lusters, but no one that I'm aware of makes anything like the Halo.

A real shame, because it was a great product.

Re: halo lustre

Posted: Fri Sep 20, 2013 11:59 pm
by Bert Weiss
I would ask if Hereaus is making it. They are currently in the Lustre business. They bought Engelhard from BASF in 2009. I see no mention of halo, but they do do marble.
http://heraeus-preciouscolours.de/media ... =125853006

Re: halo lustre

Posted: Sat Sep 21, 2013 8:04 am
by Brad Walker
I asked Heraeus a while back and they said they weren't making a Halo product. That may have changed, but I have my doubts.

Re: halo lustre

Posted: Sat Sep 21, 2013 8:52 am
by Bert Weiss
Brad Walker wrote:I asked Heraeus a while back and they said they weren't making a Halo product. That may have changed, but I have my doubts.
Do we have any chemists in the house who can figure out how to alter an available lustre to do the halo thing?

Re: halo lustre

Posted: Sat Sep 21, 2013 9:58 pm
by Barb R
I just googled it - and am not sure if this is the same thing, but try:

http://www.seattlepotterysupply.com/Mer ... ode=HHLAHM

Barb