Fusing 19" dia. dichroic sheet to clear SPE 96
Moderators: Brad Walker, Tony Smith
Fusing 19" dia. dichroic sheet to clear SPE 96
How do I avoid trapping air bubbles when fusing this size material?
-
- Site Admin
- Posts: 1528
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Fusing 19" dia. dichroic sheet to clear SPE 96
See this thread: http://www.warmglass.com/phpBB/viewtopi ... =2&t=40939BobAde wrote:How do I avoid trapping air bubbles when fusing this size material?
One additional comment -- if you fuse with the dichroic on top, you will have more trapped air bubbles than if you fuse with a thicker glass on top. That's because the thicker glass will help to push bubbles out.