Re: Devit Problem with BE
Posted: Fri Dec 20, 2013 10:45 pm
this is b.e. steel blue. it's not devit, nor is it the thinfire. at the temps he's using, it's starting to develop the normal silvery gray coating that the steel blues (opal, transparent) develop. capping with clear is the solution.