hire fire glue?
Moderators: Brad Walker, Tony Smith
-
Babette (Shawn)
- Posts: 103
- Joined: Fri Feb 05, 2010 4:11 pm
- Location: Chico California
- Contact:
hire fire glue?
Is there any glue that will hold glass together at slumping temperatures? I slump at about 1100F.
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
― Pablo Picasso
-
Terry Curtis
- Posts: 15
- Joined: Tue Apr 04, 2006 9:26 pm
- Location: Goffstown, NH
- Contact:
Re: hire fire glue?
what are you trying to do? Are you trying to avoid an extra firing instead of first doing a tack fuse and then slumping?
Terry Curtis
Re: hire fire glue?
i doubt it. most glues are organic, and organics can't usually last that high. there may be some hi-temp epoxies; for instance, you can use some epoxies on car headers, which probably reach 800-900F or so.