Posted: Sun Feb 02, 2014 9:12 pm
by susanmozingo
I can score and break 3mm Tetka without a problem. I break using either the Morton button or running pliers. If the piece of Tetka is thicker than 3MM I can't break the score. Do I need to press harder when I am scoring? Thanks.
Re: Tetka thicker than 3MM
Posted: Sun Feb 02, 2014 10:36 pm
by Marty
Don't score any harder.
You will need slightly more breaking pressure for the 4mm and considerably more for the 6mm.
Get yourself these for the 6mm:
http://shop.bullseyeglass.com/tools-sup ... liers.html
I'm not sure about other (cheaper) sources for those, you'll have to do some research.
Re: Tetka thicker than 3MM
Posted: Sun Feb 02, 2014 11:00 pm
by susanmozingo
Thank you