drilling holes in glass
I have been using CR Laurence standard plated diamond drills for drilling holes in fused glass lampshades. I spend about $35-$40 on the drill bit, and it seems to last for about 5 holes. Anyone have a better source for a drill bit that lasts longer? The next step up at CR Laurence is about $130. Sheesh...
Thanks!
Thanks!
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: drilling holes in glass
Well, you only need to drill 15 holes with the more expensive bit and you have paid for it.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: drilling holes in glass
Are the CRL bits sintered or plated? Sintered bits will last a lot longer. You might check out HIS Glassworks and see if they have something that will work well for you, I know that they do carry sintered bits.kristyslyglass wrote:I have been using CR Laurence standard plated diamond drills for drilling holes in fused glass lampshades. I spend about $35-$40 on the drill bit, and it seems to last for about 5 holes. Anyone have a better source for a drill bit that lasts longer? The next step up at CR Laurence is about $130. Sheesh...
Thanks!
-
Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: drilling holes in glass
I buy all my bits from http://thk.hk/index.php
they come from hong kong and work just as well as the ones you are getting from CRL
For example here are three 1" bits for $6.80... yes around $2.20 each and the shipping is only $4.00

http://thk.hk/onlinestore_details.php?id=1
You will get as much or more use out of one of these than the CRL cheap ones.
they come from hong kong and work just as well as the ones you are getting from CRL
For example here are three 1" bits for $6.80... yes around $2.20 each and the shipping is only $4.00
http://thk.hk/onlinestore_details.php?id=1
You will get as much or more use out of one of these than the CRL cheap ones.
Rick Wilton
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: drilling holes in glass
I haven't looked on CRL for bits in a while. I used to buy the Amazing Glazing line, which cost more than their cheapest, and less than their most expensive. Those last a lot longer and can be dressed.
I bought some like Rick suggests, and they are useless to me. The shanks are so short that the bit doesn't reach the glass using my tripod drill. I tried to buy an extension, but the American sized extensions are too small. I couldn't find any metric ones.
I bought some like Rick suggests, and they are useless to me. The shanks are so short that the bit doesn't reach the glass using my tripod drill. I tried to buy an extension, but the American sized extensions are too small. I couldn't find any metric ones.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: drilling holes in glass
You might also look at your drilling workflow. Could be that you're heating up the bit more than necessary?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
-
Tom Fuhrman
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
Re: drilling holes in glass
chek out lopacki.com I've used his stuff for many years.
Re: drilling holes in glass
In the Puget Sound area there is a company called ConCut that can supply drill bits and saw blades. We did a tour of their facility about 7 years ago. It was very interesting and they are great to work with.
KaCe
KaCe
-
Michele gh
- Posts: 71
- Joined: Tue Sep 21, 2004 11:10 pm
- Location: Massachusetts
- Contact:
Re: drilling holes in glass
I bought Amico 12 mm (.5 inch) bits - 2 bits for $8 from Amazon. I used them to drill through glass electrical insulators (about .5 inch thick glass). I got 10 holes out of one bit. I built a damn with plumbers putty around the area I wanted to drill, and filled the damn with Stained Glass Grinder Coolant mixed with water per the bottle's instructions. When I drilled I took short strokes, then brought the bit up into the Coolant solution in an attempt to keep my bit cool, then took another short stroke at drilling, until my bit broke through the glass. My drill speed was set at 2000 rpm.
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: drilling holes in glass
Daniel Lopacki is a good source,
Also check out ebay seller LAU*** (yep that's correct). Great prices and good quality.
Also check out ebay seller LAU*** (yep that's correct). Great prices and good quality.
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: drilling holes in glass
Just checked out Rick's ,
It is the online store for LAU***
Great minds......
It is the online store for LAU***
Great minds......
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns