kiln board
Posted: Thu Apr 03, 2014 9:59 am
				
				I'm looking for a kiln board that I can fuse onto that hopefully does not need fibre paper, which I find uncomfortable to be around.
I've got a white 2" thick board that seems to have rigidizer on it, but a section of it got pulled away from a previous casting. I also have a vermiculite board about 2" thick, but it needs to be surfaced with something...It is 18" wide - ideally I'd like something about 24" wide by 36" long ( or could use a couple of pieces to butt together.)
Is a stainless steel sheet on top of one of these a decent answer for longevity,and not needing a fibre paper? Can I sand flat the white board with a belt sander, and re-rigidize the surface? I'd want to have the board remain flat.
Looking to make some grit casting sheets, but have to get a good surface to begin with....
			I've got a white 2" thick board that seems to have rigidizer on it, but a section of it got pulled away from a previous casting. I also have a vermiculite board about 2" thick, but it needs to be surfaced with something...It is 18" wide - ideally I'd like something about 24" wide by 36" long ( or could use a couple of pieces to butt together.)
Is a stainless steel sheet on top of one of these a decent answer for longevity,and not needing a fibre paper? Can I sand flat the white board with a belt sander, and re-rigidize the surface? I'd want to have the board remain flat.
Looking to make some grit casting sheets, but have to get a good surface to begin with....