What's the difference between clear frit and water clear frit?
Re: Clear frit
different glasses. water clear is more transparent than clear.
Re: Clear frit
Usually the water clear (or crystal clear) is more colorless than the regular clear. It can make a difference, especially when you're mixing colors. Otherwise, they're pretty much interchangeable.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Clear frit
You can really tell the difference if your piece is fairly thick as in a casting.