I have some glass that by a slight chance might be Vaseline glass I can't seem to locate a black light to check it out . I would like to use it in some pod molds and was wondering if there were any hazards I should be aware of either to me or the kiln.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: vasoline glass

Post by Brad Walker »

No hazards. The uranium oxide is totally contained.
Thomas Decker
Posts: 24
Joined: Thu Feb 17, 2011 11:26 pm

Re: vasoline glass

Post by Thomas Decker »

THANKS.
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: vasoline glass

Post by Judd »

My experiments were not pleasing. It fused like float.
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: vasoline glass

Post by Greg Rawls »

What is vasoline glass?
Greg
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: vasoline glass

Post by Brad Walker »

Greg Rawls wrote:What is vasoline glass?
Also, known as uranium glass, it's glass that is made with a small amount of uranium oxide. That makes it glow under a black light. It was really popular around the 30's, but stopped being widely made after WWII, when uranium was used for other things. :)

Today you mostly find it in some boro (for pipes) and marbles (glow in the dark). There was a company making some for fusing a few years ago, but I don't know if they're still around.

Called Vaseline glass because that's the color.