coldworking mirror--like regular glass?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

coldworking mirror--like regular glass?

Post by Nina Falk »

I want to cut some mirror and cold work the edges. Anything I should know?
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: coldworking mirror--like regular glass?

Post by Bert Weiss »

The glass is regular float. The backing is regular paint.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: coldworking mirror--like regular glass?

Post by Nina Falk »

I know that. will it behave any differently with wet belt/grinder?
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: coldworking mirror--like regular glass?

Post by charlie »

no, except the silvering or paint may chip on the edges. use a very fine grit head on your grinder and belts.
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: coldworking mirror--like regular glass?

Post by Nina Falk »

thanks. I will.
Vonon
Posts: 196
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: coldworking mirror--like regular glass?

Post by Vonon »

Nina, I can hardly wait to see what you're doing with mirrors. I hope its nothing practical.
Vonon
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: coldworking mirror--like regular glass?

Post by Nina Falk »

let me reflect on a reply..
Vonon
Posts: 196
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: coldworking mirror--like regular glass?

Post by Vonon »

:lol: Nina, you never disappoint!
Vonon
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: coldworking mirror--like regular glass?

Post by Buttercup »

Nina, if you're bonding it to other glass or a substrate make sure you use an appropriate bonding agent. Some eat the silvering. Sorry I can't come up with a North American brand name right now but someone will know. Jen
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: coldworking mirror--like regular glass?

Post by Nina Falk »

it is far more humble..just for a base for my glass. I just want to customize the size/shape of the mirror.
Mark Hall
Posts: 59
Joined: Sun Mar 23, 2003 11:11 pm
Location: Kasota, MN
Contact:

Re: coldworking mirror--like regular glass?

Post by Mark Hall »

FYI, scratching out a design on the backside of a mirror then slumping into shape produces interesting results. Often the paint comes off leaving the silver layer intact (my favorite tool for this is a razor blade). Modern day electro-plated mirrors react differently than old-time poured silver w/ bituminus applied paint. Fired mirror results often varies in color; pink, yellow, black - and I haven't been able to control that.
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: coldworking mirror--like regular glass?

Post by Nina Falk »

thanks for sharing your experiments, Mark!
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: coldworking mirror--like regular glass?

Post by Buttercup »

Carefully controlled sandblasting will remove the paint if you can stop before removing the 'silvering'.

Mark, would there be any toxic fumes from the heated silvering? I just looked it up and the modern coating seems to be aluminum. How safe is that? Jen
Mark Hall
Posts: 59
Joined: Sun Mar 23, 2003 11:11 pm
Location: Kasota, MN
Contact:

Re: coldworking mirror--like regular glass?

Post by Mark Hall »

Safe? I'm more concerned about all the aluminum used in most deoderants, or cooking in aluminum pans than backs of mirrors!
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: coldworking mirror--like regular glass?

Post by Buttercup »

The undisturbed aluminum on the items you mention won't enter your lungs. I'm not an expert, don't even have anything to base my question on other than evidence of the damage that other normally-inert substances can do if heated and inhaled. Being curious I Googled 'neurotoxicity of aluminum fumes'. Try it. Jen
Mark Hall
Posts: 59
Joined: Sun Mar 23, 2003 11:11 pm
Location: Kasota, MN
Contact:

Re: coldworking mirror--like regular glass?

Post by Mark Hall »

I guess we're a bit off topic discussing warm working mirror instead of cold working, but it's all relevant to our trade. I did google toxicity of aluminum and there is some evidence it may be harmful but the jury is still out on this. However, I suspect many substrates we apply to glass then fire may be harmful to some degree. Burning off copper-plated backing or any kind of organic paint can't be good to breathe. I would certainly not want my kiln near my living quarters such as in the basement or attached garage. If in doubt, I'll start the program at the end of the day leaving the spiders to deal with the fumes. It's not something done regularly so it's not too different than all the other dangers we face every day.