When is safe to blast?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

When is safe to blast?

Post by Bonnie Rubinstein »

When is it safe to blast the back of a piece that has just finished cooling to room temp? Is it at risk to bast, i.e. in 2 hours ?

thanks!
Bonnie Rubinstein
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: When is safe to blast?

Post by DonMcClennen »

If it is room temp then your good to go!
"The Glassman"
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: When is safe to blast?

Post by Tony Smith »

Hi Bonnie!

What Don said.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: When is safe to blast?

Post by Bonnie Rubinstein »

Hi Tony! hope all is well!

Thanks, guys.. I was under the gun(pardon the pun!).. so I went and did the deed, and it is fine.

phew! had 36 hrs. to create a complicated piece..feel like I just took a final exam, like both my daughters!
Bonnie Rubinstein
Post Reply